Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 98.2 MPa | 14200 psi | ASTM D3759 |
3M 850 Polyester Film Tape 3M™ Polyester Film Tape 850 can generally be used for splicing and applications where chemical resistance and/or clean removal is necessary. The silver backing is a transparent polyester with a thi.. |