Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 9.79 MPa | 1420 psi | |
Shin-Etsu Silicones FEA-251U Fluorosilicone Elastomer ShinEtsu FEA251 U is one of a series of fluorosilicone compounds. It is designed to process well in molding applications. It can be blended with other members of the series for intermediate hardness.. |
|||
Tensile Strength at Break | 9.79 MPa | 1420 psi | ASTM D638 |
Teknor Apex Telcar® 95-T0769V-90NT Ethylene Vinyl Acetate Copolymer Notes: The Specialty Compounding Division offers a proprietary line of cap-liner compounds designed for carbonated soft drinks. These are proven products that have been used commercially for several.. |
|||
Tensile Strength at Break | 9.79 MPa @Thickness 1.91 mm |
1420 psi @Thickness 0.0750 in |
20 in/min; ASTM D412 |
Teknor Apex Telcar® TL-1934F Styrenic Thermoplastic Elastomer Notes: RoHS Compliant Uses: Appliance Wire Insulation; Cable Jacketing; Flexible Cord Insulation; Connectors; Wire Jacketing Agency Ratings: UL 1581Forms: Pellets Processing Method: Extrusion; Injec.. |
|||
Tensile Strength at Break | 9.79 MPa | 1420 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 8201-80 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a w.. |
|||
Tensile Strength at Break | 9.79 MPa | 1420 psi | |
Aearo E-A-R Specialty Composites Isoloss® HD Polyurethane Elastomer Isoloss® Polyurethane Elastomers feature high internal damping properties for low amplification at resonance to protect equipment during frequency cycling and random shocks, effective shock protect.. |
|||
Tensile Strength at Break | 9.79 MPa | 1420 psi | ISO 37 |
Alliance Polymers Viprene™ G80A-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G80A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Strength at Break | 9.79 MPa | 1420 psi | ISO 37 |
Alliance Polymers Viprene™ G80A-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G80A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |