Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 9.03 MPa @Temperature 23.0 °C |
1310 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versaflex™ FFC 2882-87 Thermoplastic Elastomer (TPE) Versaflex™ FFC 2882-87 is designed to pass several fatty food extraction conditions identified in EU Directive 2002/72/EC, FDA 21 CFR 177.2600, and GB 4806.1-94. Versaflex™ FFC 2882-87 will also o.. |
|||
Tensile Strength at Break | 9.03 MPa | 1310 psi | Across Flow; ASTM D412 |
ExxonMobil Geolast® 701-87W183 Thermoplastic Elastomer A hard, black, oil resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good hot air and hot oil resistance for use in a wide range of applic.. |
|||
Tensile Strength at Break | 9.03 MPa | 1310 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 251-80W232 Thermoplastic Elastomer A soft, colorable, flame retardant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material has good fluid resistance and contains non-ether brominated flame retard.. |
|||
Tensile Strength at Break | 9.03 MPa | 1310 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 8221-85M300 Thermoplastic Elastomer A hard, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is designed for automotive interior applications requiring low fogging and .. |