Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 8.96 MPa | 1300 psi | TM R050-36 |
Resinlab® EP1225 Black Unfilled Epoxy Adhesive Resinlab™ EP1225 Black is a two part unfilled epoxy adhesive designed for bonding of metals, ceramics and most plastics. It has slightly thixotropic viscosity to give gap filling ability bust stil.. |
|||
Tensile Strength at Break | 8.96 MPa | 1300 psi | 51 mm/min; ASTM D638 |
PolyOne Maxxam™ FR WC-P85 NHFR RoHS Natural Polyolefin, Unspecified Maxxam™ HFFR WC-P85 RoHS Natural is a halogen-free flame retardant polyolefin compound characterized by low smoke, low flame spread, excellent spring-back, no plate-out and high extrusion line spee.. |
|||
Tensile Strength at Break | 8.96 MPa | 1300 psi | ASTM D412 |
Teknor Apex APEX® 3060-H Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Good FlexibilityUses-General Purpose, ProfilesAppearance-Natural Color, OpaqueForms-PelletsProcessin.. |
|||
Tensile Strength at Break | 8.96 MPa | 1300 psi | ASTM D412 |
Teknor Apex Monprene® MP 1023 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 8.96 MPa | 1300 psi | ASTM D412 |
Teknor Apex Monprene® MP 1851 Thermoplastic Elastomer Notes: Translucent Features: High FlowInformation Provided by Teknor Apex |
|||
Tensile Strength at Break | 8.96 MPa | 1300 psi | ASTM D412 |
Teknor Apex Monprene® MP-1848 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 8.96 MPa | 1300 psi | ASTM D412 |
Teknor Apex Monprene® MP 1304S Thermoplastic Elastomer Uses: Grips Features: Good Resistance to Skin OilsInformation Provided by Teknor Apex |
|||
Tensile Strength at Break | 8.96 MPa | 1300 psi | ASTM D412 |
Teknor Apex Monprene® MP 1564 Thermoplastic Elastomer Notes: Translucent Features: High FlowInformation Provided by Teknor Apex |
|||
Tensile Strength at Break | 8.96 MPa | 1300 psi | ASTM D412 |
Teknor Apex Monprene® MP-2579A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 8.96 MPa | 1300 psi | ASTM D412 |
Teknor Apex Monprene® MP-2581A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 8.96 MPa | 1300 psi | ASTM D412 |
Teknor Apex Monprene® MP-2850M Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 8.96 MPa | 1300 psi | ASTM D412 |
Teknor Apex Monprene® MP-3017 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 8.96 MPa | 1300 psi | ASTM D412 |
Teknor Apex Telcar® OBC 4665A Thermoplastic Elastomer Uses: Blow Molding Applications; General Purpose; Soft Touch Applications Forms: Pellets Processing Method: Blow Molding; Profile Extrusion; Sheet Extrusion; Thermoforming; Wire and Cable Extrusion;.. |
|||
Tensile Strength at Break | 8.96 MPa | 1300 psi | ASTM D412 |
Teknor Apex Telcar® TL-1137 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Strength at Break | 8.96 MPa | 1300 psi | ASTM D412 |
Teknor Apex Telcar® TL-1642E Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Strength at Break | 8.96 MPa | 1300 psi | ASTM D412 |
Teknor Apex Uniprene® UN-7010-87NT Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Gaskets; Glazing; Grommets; Medical Pump Seals; Medical/Healthcare Applications; Plugs; Shock Absorbing Pads; Tubing Agency Ratings: NSF 61 Forms: Pellets Processin.. |
|||
Tensile Strength at Break | 8.96 MPa | 1300 psi | ASTM D638 |
ExxonMobil HDPE HD 6706.17 High Density Polyethylene Copolymer Resin Product Description: HD 6706 is a narrow molecular weight hexane copolymer designed for good processability and excellent balance of ESR, Toughness and Stiffness properties. This resin is ideally su.. |
|||
Tensile Strength at Break | 8.96 MPa | 1300 psi | ASTM D638 |
ExxonMobil HDPE HD 6706.62 High Density Polyethylene Copolymer Resin Product Description: HD 6706 is a narrow molecular weight hexane copolymer designed for good processability and excellent balance of ESR, Toughness and Stiffness properties. This resin is ideally su.. |
|||
Tensile Strength at Break | 8.96 MPa | 1300 psi | ISO 527-2/1A/50 |
ExxonMobil LDPE LD 600BA Low Density Polyethylene Resin (European Grade) Product Description: LD 600BA is a high flow LDPE grade, characterized by high stiffness and good toughness. It’s easy processable.Availability: Africa & Middle East and Europe Additive: Antiblock.. |
|||
Tensile Strength at Break | 8.96 MPa | 1300 psi | ASTM D638 |
Entec Hypel® PELD50/.924 LDPE Available in North America Features: Food Contact Acceptable and Low DensityAgency Ratings: FDA 21 CFR 176.170, Table 2, Cond. B; Cond. C; Cond. D; Cond. E; Cond. F; Cond. G; Cond. H; and FDA 21 CF.. |
|||
Tensile Strength at Break | 8.96 MPa | 1300 psi | Molded and tested in accordance with ASTM D4976; ASTM D638 |
Dow DNDA-1149 NT 7 Linear Low Density Polyethylene Resin DOW DNDA-1149 NT 7 is produced using UNIPOL™ PE process technology and is intended for high-speed injection molding applications. Information provided by Dow |
|||
Tensile Strength at Break | 8.96 MPa | 1300 psi | ASTM D412 |
DuPont Performance Polymers Kalrez® Spectrum™ 0040 Fluoroelastomer Kalrez® Spectrum™ 0040 perfluoroelastomer parts are specifically designed for low-temperature environments where significant chemical resistance is required. Proprietary polymer and cure technolog.. |
|||
Tensile Strength at Break | 8.96 MPa | 1300 psi | ASTM D638 |
ExxonMobil Escorene™ LD 706.15 Molding Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra LD 706.15 is a 14.9 wt% vinyl acetate copolymer film resin designed for specialty molding, extrusion and compounding applications.Availability: Latin America, Nor.. |
|||
Tensile Strength at Break | 8.96 MPa | 1300 psi | ASTM D412 |
Teknor Apex Monprene® MP 1037 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 8.96 MPa | 1300 psi | ASTM D412 |
Teknor Apex Monprene® MP-2875M Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 8.96 MPa | 1300 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 221-87W211 Thermoplastic Elastomer
(discontinued **) A hard, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide.. |