Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 8.50 MPa | 1230 psi | ISO 37 |
PolyOne OnFlex™ S FR 80A-3S1892 Thermoplastic Elastomer (TPE) OnFlex™-S FR thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially flame retarded with a highly effective, RoHS compliant halo.. |
|||
Tensile Strength at Break | 8.50 MPa | 1230 psi | ASTM D638 |
Petroquimica Triunfo Trithene® CX 7065 LDPE - Extrusion Coating The Trithene® CX 7065 resin is a product developed especially to meet the segment of extrusion coating where the following properties are necessary: processing stability at high production rates, a.. |
|||
Tensile Strength at Break | 8.50 MPa | 1230 psi | ASTM D638 |
Petroquimica Triunfo Trithene® JX 7065 LDPE - Injection Molding and Master Batch The Trithene® JX 7065 resin is a low-density polyethylene with a wide molecular weight distribution, developed to offer good impact resistance, excellent flexibility, and high resistance to stress .. |
|||
Tensile Strength at Break | 8.50 MPa | 1230 psi | ASTM D638 |
UBE J3519 Polyethylene Description: UBE Polyethylene is polymerized at high pressure using a tubular reactor. Production conditions are strictly controlled ensuring the product's superior physical and mechanical prope.. |
|||
Tensile Strength at Break | 8.50 MPa | 1230 psi | ISO 37 |
ELASTO UK Dryflex® 3031-102 TPE, Modified Injection Molding Grade for Auto Interior Parts The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. VTC Dryflex® 3031-102 is specifically designe.. |
|||
Tensile Strength at Break | 8.50 MPa | 1230 psi | ISO 527-1 |
Barlog Plastics KEBAFLEX SG 75 A.1 black TPE-S, Shore A75, black TPE-SInformation provided by BARLOG plastics GmbH. |
|||
Tensile Strength at Break | 8.50 MPa | 1230 psi | ISO 527-1 |
Barlog Plastics KEBAFLEX SG 75 A.1 TPE-S, Shore A70, natural TPE-SInformation provided by BARLOG plastics GmbH. |