Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 7.79 MPa | 1130 psi | ASTM D412 |
Teknor Apex Monprene® MP-1358C Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 7.79 MPa | 1130 psi | ASTM D412 |
Teknor Apex Telcar® TL-3954-90 Thermoplastic Elastomer Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Insulation; Terminal Cable Jacketing; Underground Power Cable; Wire .. |