Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 7.58 MPa @Temperature 23.0 °C |
1100 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G2755C Thermoplastic Elastomer (TPE) Dynaflex™ G2755C is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Good Ozone and UV Stability - Overmold Adhesion to Polypropylene .. |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | ASTM D638 |
ExxonMobil LD 509.48 Compounding Resin
(discontinued **) LD 509.48 is a high melt index homopolymer resin designed to provide good processability in compounding applications.Information provided by ExxonMobil Chemical |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible B5500 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible B550B Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | |
Shin-Etsu Silicones KE-5560U Low Temperature Silicone Elastomer ShinEtsu KE5560 U is a nominal 60 Durometer phenyl (PVMQ) base.Product Features: This material was designed for its excellent vibration dampening characteristics. Because of its phenyl content, it a.. |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | |
Shin-Etsu Silicones KE-961U Silicone Elastomer KE961 U is one of a series of easy processing, general purpose silicone rubber bases. It can be used in a variety of applications requiring finishing by molding (compression, injection, transfer).Pr.. |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | ASTM D412 |
Teknor Apex Monprene® MP 1843L1 Thermoplastic Elastomer Notes: Translucent Features: High FlowInformation Provided by Teknor Apex |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | ASTM D412 |
Teknor Apex Monprene® MP 1627L3 Thermoplastic Elastomer Features: Excellent Elastic Recovery; Tough; Good Melt Strength Uses: Strap ProductsInformation Provided by Teknor Apex |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | ASTM D412 |
Teknor Apex Monprene® MP 1875 Thermoplastic Elastomer Notes: Water; Clear; Adhesion to Polycarbonate Features: High Coefficient of FrictionInformation Provided by Teknor Apex |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | ASTM D412 |
Teknor Apex Monprene® MP-1627 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | ASTM D412 |
Teknor Apex Monprene® MP 1504 Thermoplastic Elastomer Notes: Translucent Features: Tough; Good Melt Strength Uses: Safety ProductsInformation Provided by Teknor Apex |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | ASTM D412 |
Teknor Apex Monprene® MP-2432F Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | ASTM D412 |
Teknor Apex Monprene® MP-2780 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | ASTM D638 |
Teknor Apex Telcar® 90-E607D-88NT Ethylene Vinyl Acetate Copolymer Notes: The Specialty Compounding Division offers a proprietary line of cap-liner compounds designed for carbonated soft drinks. These are proven products that have been used commercially for several.. |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | ASTM D412 |
Teknor Apex Telcar® TL-1050-75 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | ASTM D412 |
Teknor Apex Telcar® TL-1336G Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | ASTM D412 |
Teknor Apex Telcar® TL-2560A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | ASTM D412 |
Teknor Apex Telcar® TL-2590F Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | ASTM D638 |
ExxonMobil LD 516.LN Molding, Extrusion and Compounding Resin Product Description: LD 516.LN is a medium MI, low density polyethylene resin designed for use in color concentrates and masterbatches where its flow properties ensure improved processability and un.. |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | ASTM D638 |
ExxonMobil LD 637.LI Molding, Extrusion and Compounding Resin Product Description: LD 637.LI is a high melt index LDPE homopolymer intended for injection molding or compounding applications requiring high flow. It is ideal for tamper-evident, tear-to-open clos.. |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | ASTM D638 |
ExxonMobil LDPE LD 617.LN Low Density Polyethylene Resin Product Description: LD 617.LN is a high flow, low density polyethylene homopolymer resin designed to provide excellent processability, flexibility and surface appearance. This multipurpose resin is.. |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | ASTM D638 |
ExxonMobil LDPE LD 637.LI Low Density Polyethylene Resin Product Description: LD 637.LI is a high melt index LDPE homopolymer intended for injection molding or compounding applications requiring high flow. It is ideal for tamper-evident, tear-to-open clos.. |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | ASTM D638 |
ExxonMobil LLDPE LL 5252.09 Linear Low Density Polyethylene Resin Product Description: LL 5252.09 is a linear low density polyethylene resin designed to provide good processability and ease of blending. The granular from of LL 5252.09 makes for efficient blending .. |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | ASTM D412 |
Teknor Apex Monprene® MP-1875HF Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 7.58 MPa | 1100 psi | ASTM D412 |
Teknor Apex Monprene® MP-2770 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |