Polymer Property : Tensile Strength at Break = 7.205 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 7.205 MPa

@Time 7200 sec
1045 psi

@Time 2.00 hour
Die C; ASTM D414
STAR Thermoplastic Alloys & Rubbers StarTUFF TF 65-HR-9 TPE
Product Description: StarTUFF TF 65-HR-9 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelHigh Tear strengthHigh Tensile strengthProcessing Method: Injection M..