Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 66.7 MPa | 9670 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® NH-1021 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Tensile Strength at Break | 66.7 MPa | 9670 psi | ASTM D638 |
Unitika elitel UE3210 Polyester, Pellet Medium Tg, standard resin, BinderUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from products such as adhesives, paints, ink bi.. |
|||
Tensile Strength at Break | 66.7 MPa | 9670 psi | ASTM D3759 |
3M 855 High Temperature Nylon Tape 3M™ High Temperature Nylon Tape 855 is a 2 mil nylon film tape with a non-silicone rubber adhesive that can be used in many composite bagging operations or to help remove flashing after composite b.. |
|||
Tensile Strength at Break | 66.7 MPa | 9670 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® NH-1021 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |