Mechanical Properties Metric English Comments
Tensile Strength at Break >= 645 MPa
>= 93500 psi
14.4 lb. Minimum Tensile Load 0.014 in. Diameter
Shakespeare FL-8 Fluorocarbon PVDF Fishing Line, 12 lb
100% pure PVDF fluoro-polymer, great clarity, limpness and strength, low refractive index that decreases the visibility of the line.Information provided by Shakespeare Company.
Tensile Strength at Break >= 645 MPa
>= 93500 psi
90 lb. Minimum Tensile Load 0.035 in. Diameter
Shakespeare NX-806 Saltwater Nylon Copolymer Fishing Line, 80 lb
Low stretch, high knot strength, shock strength, abrasion resistance, superior clarity.Information provided by Shakespeare Company.
Tensile Strength at Break >= 645 MPa
>= 93500 psi
4.7 lb. Minimum Tensile Load 0.008 in. Diameter
Shakespeare S-3 Economy Nylon Copolymer Fishing Line, 4 lb
Information provided by Shakespeare Company.
Tensile Strength at Break 645 MPa
93500 psi
3.6 lb. load and 0.007 in. diameter
Shakespeare WonderThread® SN-38 High tenacity TEX# 27 Nylon Industrial Sewing Thread
Used for sewing: Bedspreads, Comforters, Caps, Hats, Blankets, Stuffed Toys, Pillows, Carpets and Rugs, Handbags, Indoor Furniture, Curtains and Drapes, Apparel, Sleeping BagsInformation provided b..
Tensile Strength at Break 645 MPa

@Temperature 870 °C,
Time 1.80e+6 sec
93500 psi

@Temperature 1600 °F,
Time 500 hour
Room Temperature properties after Isothermal Exposure
Special Metals INCOLOY® alloy 803 Fe-Ni-Cr Alloy
INCOLOY® alloy 803 (UNS S35045), an iron-nickel-chromium alloy, is designed for use in petrochemical, chemical and thermal processing applications. The nickel and chromium contents of alloy 803 ar..
Copyright © lookpolymers.com All Rights Reserved