Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 621 MPa | 90000 psi | High Speed Steel (18 W, 4 Cr, 1 V) butt joint |
Lucas-Milhaupt EASY FLO 45 Silver Based Cadmium-Bearing Filler Metal Applications: Easy-Flo 45 is very versatile and can be used successfully on nearly all nickel, iron and copper base alloys. In certain instances, special fluxes, may be required to obtain good wet.. |
|||
Tensile Strength at Break | 621 MPa | 90000 psi | Hard |
California Fine Wire Copper Clad 1006 Steel (40% Conductivity) All values may vary dependent on specific design and usage1006 steel core, 99.99% copper cladCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Tensile Strength at Break | 621 MPa | 90000 psi | Stress relieved |
California Fine Wire Nickel Alloy 99 All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Tensile Strength at Break | 621 MPa | 90000 psi | Stress relieved |
California Fine Wire Nickel Alloy 99 Nickel Alloy All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Tensile Strength at Break | 621 MPa | 90000 psi | Annealed |
California Fine Wire Stablohm 610 Nickel, Chromium and Iron Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Tensile Strength at Break | 621 MPa | 90000 psi | Annealed |
California Fine Wire Stablohm 750 Chromium, Aluminum, and Iron Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Tensile Strength at Break | 621 MPa | 90000 psi | Annealed |
California Fine Wire Stablohm 825 Nickel Chromium Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Tensile Strength at Break | >= 621 MPa | >= 90000 psi | |
Carlson 2205 (UNS S31803) Duplex Stainless Steel General DescriptionCarlson Alloy 2205 is a second-generation, nitrogen-alloyed duplex stainless steel (ferritic-austenitic). It offers an excellent combination of both strength and corrosion resist.. |
|||
Tensile Strength at Break | >= 621 MPa | >= 90000 psi | |
Carlson 2205 (UNS S32205) Duplex Stainless Steel General DescriptionCarlson Alloy 2205 is a second-generation, nitrogen-alloyed duplex stainless steel (ferritic-austenitic). It offers an excellent combination of both strength and corrosion resist.. |