Polymer Property : Tensile Strength at Break = 6.87 MPa
Polymer Property :
Tensile Strength at Break =
6.87 MPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
6.87
MPa
996
psi
Shin-Etsu Silicones KE-661U Silicone Elastomer
Information Provided by Shin-Etsu Silicones of America, Inc.