Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 6.00 MPa | 870 psi | ISO 37 |
PolyOne OnFlex™ S FR 50A-3S1831 Thermoplastic Elastomer (TPE) OnFlex™-S FR thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially flame retarded with a highly effective, RoHS compliant halo.. |
|||
Tensile Strength at Break | <= 6.00 MPa | <= 870 psi | ISO/R527 |
Polykemi AB POLYelast TPE E706 Thermoplastic Elastomer, EPDM-based Information provided by Polykemi AB |
|||
Tensile Strength at Break | 6.00 - 10.0 MPa | 870 - 1450 psi | |
Prodways PLASTCure Flex 100 3D Printing Polymer High workability. Meet criteria regarding irritation, sensitisation and cytotoxicity for biological assessment of medical products (DIN ISO 10993)Suitable for the manufacture of flexible objects for.. |
|||
Tensile Strength at Break | 6.00 MPa | 870 psi | ASTM D412 |
Teknor Apex Telcar® TL-1035-70 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Strength at Break | 6.00 MPa | 870 psi | ASTM D412 |
Teknor Apex Telcar® TL-1035-70UV Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Strength at Break | 6.00 MPa | 870 psi | ISO 527 |
A. Schulman INVISION™ VX-5090UI Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5090UI is a UV-stabilized thermoplastic elastomer which has been formulated for easy moldability, soft touch, low gloss, and excellent weatherability.Information provided by.. |
|||
Tensile Strength at Break | 6.00 MPa | 870 psi | ASTM D638 |
ELASTO UK Dryflex® 400801S SBS Based Material, 80A Hardness, Natural The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
Tensile Strength at Break | 6.00 MPa | 870 psi | ASTM D638 |
ELASTO UK Dryflex® 402801S SBS Based Material, 80A Hardness, Black The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
Tensile Strength at Break | 6.00 MPa | 870 psi | ASTM D638 |
ELASTO UK Dryflex® 500550S SEBS Based Material, Unfilled Qualities, 55A Hardness, Translucent The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
Tensile Strength at Break | 6.00 MPa | 870 psi | ASTM D638 |
ELASTO UK Dryflex® 502450S SEBS Based Material, Unfilled Qualities, 45A Hardness, Black The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
Tensile Strength at Break | 6.00 MPa | 870 psi | ASTM D638 |
ELASTO UK Dryflex® 502500S SEBS Based Material, Unfilled Qualities, 50A Hardness, Black The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
Tensile Strength at Break | 6.00 MPa | 870 psi | ASTM D638 |
ELASTO UK Dryflex® 602450S SEBS Based Material, Filled Qualities, 45A Hardness, Black The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Tensile Strength at Break | 6.00 MPa | 870 psi | ASTM D638 |
ELASTO UK Dryflex® 602500S SEBS Based Material, Filled Qualities, 50A Hardness, Black The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Tensile Strength at Break | 6.00 MPa | 870 psi | ASTM D638 |
ELASTO UK Dryflex® 602550S SEBS Based Material, Filled Qualities, 55A Hardness, Black The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Tensile Strength at Break | 6.00 MPa | 870 psi | ASTM D638 |
ELASTO UK Dryflex® 662550S SEBS Based Material, Semi-Filled Qualities, 55A Hardness, Black The 660-series is recommended when the properties of the produced detail requires the advantages of the 500-series in combination with the 600-series. A semi-filled material can therefore combine t.. |
|||
Tensile Strength at Break | >= 6.00 MPa | >= 870 psi | ISO R 527 |
Fainplast Compounds CR 85 Flexible PVC, Electrical Bedding Bedding |
|||
Tensile Strength at Break | >= 6.00 MPa | >= 870 psi | ISO R 527 |
Fainplast Compounds CRKA 87 Flexible PVC, Flame Retardant Electrical Bedding Lead Free Flame retardant bedding |
|||
Tensile Strength at Break | 6.00 MPa | 870 psi | ISO R 527 |
Fainplast Compounds GS 4510/R Flexible PVC, Injection Molding for Footwear Vamp Boots with Rubber |
|||
Tensile Strength at Break | 6.00 MPa | 870 psi | ASTM D638 |
ELASTO UK Dryflex® 600450S SEBS Based Material, Filled Qualities, 45A Hardness, Natural The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material .. |
|||
Tensile Strength at Break | 6.00 MPa | 870 psi | ISO 527 |
A. Schulman INVISION™ VX-5090UI Soft Touch Polyolefin Thermoplastic DescriptionInvision™ VX-5090UI is a UV-stabilized thermoplastic elastomer which has been formulated for easy moldability, soft touch, low gloss, and excellent weatherability.Information provided by.. |