Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 53.6 MPa | 7770 psi | ASTM D412 |
Huntsman IROGRAN® PS 443-201 TPU-Polyester Polyester-based grades with a broad processing window ideally suited for cast, flat die and flown film lines.Information provided by Alliance Polymers |