Polymer Property : Tensile Strength at Break = 5.94 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 5.94 MPa
861 psi
ASTM D3759
3M Scotch Pad™ 8327 Custom Carry Handle
3M™ Carry Handle 8327 is made of durable plastic strips with adhesive and each end. It is easy to create a convenient looped handle when the ends are attached to both sides of a box or package.Info..
Tensile Strength at Break 5.94 MPa
861 psi
ASTM D3759
3M Scotch Pad™ 8328 Custom Carry Handle
3M™ Carry Handle 8328 is made of durable plastic strips with adhesive and each end. It is easy to create a convenient looped handle when the ends are attached to both sides of a box or package.Info..