Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 5.17 MPa @Temperature 23.0 °C |
750 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7410-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7410-1000-00 is an easy processing, high performance compound designed for use in applications requiring a tough, durable material. - Excellent Colorability - Excellent Heat Stability - .. |
|||
Tensile Strength at Break | 5.17 MPa | 750 psi | TM R050-36 |
Resinlab® EP1295 Black Medium Viscosity, Halogen Free, Flame Retardant Epoxy Casting Resin Resinlab™ EP1295 Black is a medium viscosity, halogen free, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (.. |
|||
Tensile Strength at Break | 5.17 MPa | 750 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 121-65W233 Thermoplastic Elastomer
(discontinued **) A soft, black thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is specially formulated to bond to sulfur or peroxide-cured thermoset EPDM rubber for corner .. |
|||
Tensile Strength at Break | 5.17 MPa | 750 psi | 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible H41276D Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 5.17 MPa | 750 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible R1211P Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 5.17 MPa | 750 psi | ASTM D638 ISO 527-2 |
DuPont Elvax® 4320 Ethylene Vinyl Acetate
(discontinued **) DuPont™ Elvax® 4320 is an ethylene-vinyl acetate / acid terpolymer resin for use in industrial applications.ApplicationsElvax® 4320 resins can be used for the following applications: adhesives, s.. |
|||
Tensile Strength at Break | 5.17 MPa | 750 psi | Post oven cured 24 hours at 480°F |
Malvern Minerals Sliastic 740 with 33% Novacite® Daper Quartz Filler Press Vulcanized 5 minutes at 260° F. Product data demonstrates the effect of the Novacite® filler.Information provided by Malvern Minerals Company. |
|||
Tensile Strength at Break | 5.17 MPa | 750 psi | ASTM D412 |
Teknor Apex Monprene® MP-1277B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 5.17 MPa | 750 psi | Flow; ASTM D412 |
Teknor Apex Monprene® MP-1625A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 5.17 MPa | 750 psi | ASTM D412 |
Teknor Apex Monprene® MP-2250 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 5.17 MPa | 750 psi | ASTM D412 |
Teknor Apex Monprene® MP-1380A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 5.17 MPa | 750 psi | ASTM D412 |
Teknor Apex Telcar® TL-1138 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Strength at Break | 5.17 MPa | 750 psi | ASTM D412 |
Teknor Apex Telcar® TL-2651A Thermoplastic Elastomer Uses: Flexible Grips; Footwear; General Purpose; Grommets; Handles; Industrial Applications; Soft Touch Applications; Toys Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed.. |
|||
Tensile Strength at Break | 5.17 MPa | 750 psi | ASTM D412 |
Teknor Apex Telcar® TL-6800-64 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Strength at Break | 5.17 MPa | 750 psi | |
3M VFP-876 Tubing 3M VFP-876 is the most flexible of the heat-shrinkable, polyolefin tubings. Rated at 135°C. VFP-876 Tubing has been engineered to offer a low shrink temperature of 100°C. This allows the tubing to.. |
|||
Tensile Strength at Break | 5.17 MPa | 750 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 101-55W185 Thermoplastic Elastomer
(discontinued **) A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good fluid resistance and physical properties that meet ASTM F 477 for lo.. |