Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 46.2 MPa | 6700 psi | ASTM D638 |
Polymer Resources ABS-G10 ABS, 10% Glass Reinforced Acrylonitrile Butadiene Styrene, 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information.. |
|||
Tensile Strength at Break | 46.2 MPa | 6700 psi | ASTM D638 |
Ravago Manufacturing Americas Hylon® N1000THL Nylon 6/6 (DAM) Information provided by Ravago. |
|||
Tensile Strength at Break | 46.2 MPa | 6700 psi | ASTM D638 |
Ravago Manufacturing Americas Hylon® N1000TL Nylon 6/6 (Cond)
(discontinued **) Information provided by Ravago |
|||
Tensile Strength at Break | 46.2 MPa | 6700 psi | ASTM D638 |
Chesterton ARC S2 Ceramic reinforced erosion resistant coating Description: An advanced ceramic composite for the resurfacing and protection of all metal surfaces. It is normally applied at a thickness of 250 microns (10 mils) per coat. Non-shrinking, 100% soli.. |
|||
Tensile Strength at Break | 46.2 MPa | 6700 psi | ASTM D638 |
Chesterton MRS S2 Metal Rebuilding System An advanced ceramic composite for the resurfacing and protection of all metal surfaces. It is normally applied at a thickness of 250 microns (10 mils) per coat. Non-shrinking, 100% solids. MRS S2 is.. |
|||
Tensile Strength at Break | 46.2 MPa | 6700 psi | |
Abatron AboCast 8103-27 High-Performance Dielectric Epoxy AboCast 8103-27 is a dielectric in/outdoor epoxy system with superior arc-track resistance, high voltage and heat resistance, low ash and ion content, and it is chlorine-free. This system has high h.. |
|||
Tensile Strength at Break | 46.2 MPa | 6700 psi | ASTM D638 |
Americas Styrenics EA3400 High Heat Crystal Polystyrene Product CharacteristicsLess than 300 parts per million residual volatiles with minimal taste and odor transferExcellent clarity and colorGood toughnessFood Contact CompliantTypical ApplicationsCap l.. |
|||
Tensile Strength at Break | 46.2 MPa | 6700 psi | ASTM D638 |
Polymer Resources PC/TP-GP3 PC Polyester, High Impact, Superior Chemical Resistance
(Unverified Data**)&l Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |