Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 46.1 MPa | 6690 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® GP-5000 PBT, Unreinforced General PBT material that can be used for connectorsInformation provided by Samsung Cheil Industries. |
|||
Tensile Strength at Break | 46.1 MPa | 6690 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® GP-5000 PBT, Unreinforced General PBT material that can be used for connectorsInformation provided by Samsung Cheil Industries. |
|||
Tensile Strength at Break | 46.1 MPa | 6690 psi | 50 mm/min; ASTM D638 |
Supreme Petrochem SC 203 LV General Purpose Polystyrene CharacteristicsGood flow grade with good mechanical properties Good clarity and flexibility Easy processing grade and suitable for thin walled applicationsProcessing Extrusion MoldingApplicationsSu.. |
|||
Tensile Strength at Break | 46.1 MPa | 6690 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® LH-1070W PC, FR Information provided by Samsung Cheil Industries. |
|||
Tensile Strength at Break | 46.1 MPa | 6690 psi | 91% Ret. |
UBE UBESTA® 3030U Nylon 12 (After Ethylacetate for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Tensile Strength at Break | 46.1 MPa | 6690 psi | ASTM D3759 |
3M 34383 General Purpose Aluminum Foil Tape General purpose aluminum foil tapeInformation provided by 3M |
|||
Tensile Strength at Break | 46.1 MPa | 6690 psi | ASTM D3759 |
3M 8087 Construction Seaming Tape 3M™ Construction Seaming Tape 8087 is designed to seal seams on housewrap and insulated sheathing products. It can also be used to seam polyethylene vapor barrier products as well as to repair hole.. |
|||
Tensile Strength at Break | 46.1 MPa | 6680 psi | ASTM D638 |
Bayshore Vinyl Compounds BRC R7560 CLR 221 PVC Compound, Food Grade BRC R7560 CLR 221 is a food grade PVC bottle compound made with 100% FDA approved ingredients. This product exhibits excellent clarity and can be used in many applications where food contact is req.. |
|||
Tensile Strength at Break | 46.1 MPa | 6690 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® LH-1070W PC, FR Information provided by Samsung Cheil Industries. |