Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 445 MPa | 64500 psi | 7.3 lb. load and 0.012 in. diameter |
Shakespeare WonderThread® SN-40 ultra soft TEX# 80 Nylon Industrial Sewing Thread Used for sewing: Bedspreads, Comforters, Caps, Hats, Blankets, Stuffed Toys, Pillows, Carpets and Rugs, Handbags, Indoor Furniture, Curtains and Drapes, Apparel, Sleeping BagsInformation provided b.. |