Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 43.75 MPa | 6345 psi | ASTM D3759 |
3M 425 Aluminum Foil Tape 3M™ Aluminum Foil Tape 425 is a 5 mil nominal dead soft aluminum foil backing combined with a transparent acrylic adhesive.Information provided by 3M |
|||
Tensile Strength at Break | 43.75 MPa | 6345 psi | ASTM D3759 |
3M 427 Aluminum Foil Tape 3M™ Aluminum Foil Tape 427 is a 5 mil nominal dead soft aluminum foil backing combined with a transparent acrylic adhesive. 3M aluminum foil tape 427 offers an easy-release liner.Information provid.. |