Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 42.8 MPa | 6210 psi | ASTM D3759 |
3M 431 Premium Performance Aluminum Foil Tape Conformable aluminum tape. UL 723 ClassifiedInformation provided by 3M |
|||
Tensile Strength at Break | 42.8 MPa | 6210 psi | ASTM D3759 |
3M 5490 PTFE Extruded Film Tape 3M™ PTFE Extruded Film Tape has a film backing with a silicone adhesive.Information provided by 3M |