Polymer Property : Tensile Strength at Break = 41.7 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 41.7 MPa
6050 psi
50 mm/min; ASTM D638
Supreme Petrochem SP 243 Toughened Polystyrene
CharacteristicsGood flexibility Good clarity High stiffnessProcessing Extrusion ThermoformingApplications Clear thermoformed containers Oriented PS films LidsMaterial Status: Commercial : ActiveA..