Polymer Property : Tensile Strength at Break = 4.80 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 4.80 MPa
696 psi
Across flow; ASTM D412
Advanced Elastomer Systems Santoprene® 8281-65 Thermoplastic Rubber  (discontinued **)
Description: A colorable thermoplastic medical grade elastomer. It has USP Class VI Certificate of Compliance for biocompatibility and can be processed using injection molding, extrusion, or other ..
Tensile Strength at Break 4.80 - 6.20 MPa
696 - 899 psi
Samples die cut from pressed films, gage dimensions 2.23cm x 0.47cm x 0.13cm, crosshead speed 2in/min; ASTM D1708
DuPont Elvax® 40W Ethylene-Vinyl Acetate Copolymer Resin
Elvax® 40W has a higher vinyl acetate content compared with the other Elvax® resins resulting in higher elongation, reduced hardness, improved solubility and adhesion, and significant differences ..
Tensile Strength at Break 4.80 MPa
696 psi
Across Flow; ASTM D412 and ISO 37
ExxonMobil Santoprene® 151-70W256 Thermoplastic Vulcanizate - Flame Retardant
Product Description: A soft, black, flame retardant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material has been designed to meet the Underwriter Laboratories..
Tensile Strength at Break 4.80 MPa
696 psi
chs 20 in/min; ASTM D412
Diamond Polymers Softflex® SF 7001 Thermoplastic Vulcanizate (TPV)
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Tensile Strength at Break 4.80 MPa
696 psi
ISO 527-1
Barlog Plastics KEBAFLEX SG 50 A.1 black TPE-S, Shore A50, black
TPE-SInformation provided by BARLOG plastics GmbH.
Tensile Strength at Break 4.80 MPa
696 psi
ISO 527-1
Barlog Plastics KEBAFLEX SG 55 A.01 TPE-S, Shore A55, natural
TPE-SInformation provided by BARLOG plastics GmbH.