Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 4.10 MPa @Temperature 23.0 °C |
595 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versaflex™ OM 1060X-1 Thermoplastic Elastomer (TPE) Versaflex™ OM 1060X-1 is an overmolding TPE with very good adhesion to PC or ABS-based plastics. - Good Surface Aesthetics - Rubbery Feel - Soft Touch - Very Good Bond to PC, ABS, PC/ABSColor conce.. |
|||
Tensile Strength at Break | 4.10 MPa | 594 psi | Air at 212°F, 168 hr; ASTM D573 |
ExxonMobil Santoprene® 281-45MED Thermoplastic Elastomer
(discontinued **) A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of our medical grad.. |
|||
Tensile Strength at Break | 4.10 MPa @Time 7200 sec |
594 psi @Time 2.00 hour |
Die C; ASTM D414 |
STAR Thermoplastic Alloys & Rubbers StarCLEAR CLR-1050 TPE Product Description: StarCLEAR CLR-1050 is an easy processing TPE designed for injection molding. Soft and ultra clear TPEs specifically targeted to medical, consumer and sporting goods market. Feat.. |
|||
Tensile Strength at Break | 4.10 MPa | 595 psi | Die C; Flow direction; ASTM D412 |
Teknor Apex Sarlink® 3460 Thermoplastic Elastomer A NSF certified, low hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inject.. |
|||
Tensile Strength at Break | 4.10 MPa | 595 psi | ISO 37 |
ELASTO UK Dryflex® 3037-111 TPE, Modified Injection Molding Grade for Auto Interior Parts The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. VTC Dryflex® 3037-111 is specifically designe.. |
|||
Tensile Strength at Break | 4.10 MPa | 595 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 8191-55B100 Thermoplastic Elastomer A soft, black, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to ABS, PS, PC, PMMA, ASA, PET and PPO/PS b.. |
|||
Tensile Strength at Break | 4.10 MPa | 595 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 8211-55B100 Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to ABS, PS, PC, PMMA, ASA, PET and PPO/.. |
|||
Tensile Strength at Break | 4.10 MPa | 595 psi | ASTM D412 |
Diamond Polymers Softflex® 6001 Thermoplastic Elastomer Alloy Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength at Break | 4.10 MPa | 595 psi | Die A; ASTM D412 |
3M SJ5500 Protective Product, Molded Shapes 3M Bumpon Protective Products Molded Shapes – Colored and Clear Series are pressure-sensitive, adhesive-back polyurethane products. They can be used as feet, stops, spaces, and protectors in many a.. |
|||
Tensile Strength at Break | 4.10 MPa | 595 psi | Die A; ASTM D412 |
3M SJ5700 Protective Product, Molded Shapes 3M Bumpon Protective Products Molded Shapes – Colored and Clear Series are pressure-sensitive, adhesive-back polyurethane products. They can be used as feet, stops, spaces, and protectors in many a.. |
|||
Tensile Strength at Break | 4.10 MPa | 595 psi | Die A; ASTM D412 |
3M SJ6100 Protective Product, Molded Shapes 3M Bumpon Protective Products Molded Shapes – Colored and Clear Series are pressure-sensitive, adhesive-back polyurethane products. They can be used as feet, stops, spaces, and protectors in many a.. |
|||
Tensile Strength at Break | 4.10 MPa | 595 psi | Die A; ASTM D412 |
3M SJ5000 Protective Product, Molded Shapes 3M Bumpon Protective Products Molded Shapes – Colored and Clear Series are pressure-sensitive, adhesive-back polyurethane products. They can be used as feet, stops, spaces, and protectors in many a.. |
|||
Tensile Strength at Break | 4.10 MPa @Time 7200 sec |
594 psi @Time 2.00 hour |
Die C; ASTM D414 |
STAR Thermoplastic Alloys & Rubbers StarCLEAR CLR-1040 TPE Product Description: StarCLEAR CLR-1040 is an easy processing TPE designed for injection molding. Soft and ultra clear TPEs specifically targeted to medical, consumer and sporting goods market. Feat.. |