Mechanical Properties Metric English Comments
Tensile Strength at Break 350 MPa
50800 psi
ACMA Test #4 / DIN EN 843-1
CeramTec Rocar® SiF Silicon Carbide, SiSiC
Rocar® is an extremely lightweight silicon carbide ceramic. It permits a reduction in mass forces at high speeds, and is considered for its hardness, excellent resistance to corrosion and sudden ch..
Tensile Strength at Break >= 350 MPa
>= 50800 psi
warp
Beijing Evergrow Resources CFC-DD-1000 Carbon Fiber Cloth
The viscose yarn(cloth) are converted into carbon fiber(cloth) by the special process of weaving, preoxidization, carbonization aftertreatment etc. It has the good high temperature resistance, corro..
Tensile Strength at Break >= 350 MPa
>= 50800 psi
warp
Beijing Evergrow Resources CFC-DD-1000S Carbon Fiber Cloth
The viscose yarn(cloth) are converted into carbon fiber(cloth) by the special process of weaving, preoxidization, carbonization aftertreatment etc. It has the good high temperature resistance, corro..
Tensile Strength at Break >= 350 MPa
>= 50800 psi
warp
Beijing Evergrow Resources CFC-DDX-1000S Carbon Fiber Cloth
The viscose yarn(cloth) are converted into carbon fiber(cloth) by the special process of weaving, preoxidization, carbonization aftertreatment etc. It has the good high temperature resistance, corro..
Tensile Strength at Break >= 350 MPa
>= 50800 psi
warp
Beijing Evergrow Resources CFC-DDX-1000 Carbon Fiber Cloth
The viscose yarn(cloth) are converted into carbon fiber(cloth) by the special process of weaving, preoxidization, carbonization aftertreatment etc. It has the good high temperature resistance, corro..