Mechanical Properties Metric English Comments
Tensile Strength at Break 3.70 MPa

@Temperature 23.0 °C
537 psi

@Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Versaflex™ HC 2110-57B Thermoplastic Elastomer (TPE)
Versaflex™ HC 2110-57B is a TPE designed for use in the healthcare industry offering low stiction and good compression set. New Product. Commercial specifications have not been established. - Bonds..
Tensile Strength at Break 3.70 MPa
537 psi
ISO 37
ELASTO UK Dryflex® 8010-102 Flame Retardant TPE for Extrusion, Pebble Gray
Vitaprene® thermoplastic elastomers combine the performance of most vulcanized rubber with the process properties of thermoplastics. Vitaprene® compounds permit sophisticated component design and..
Tensile Strength at Break 3.70 MPa
537 psi
ISO 37
ELASTO UK Dryflex® 8010-102 Flame Retardant TPE for Injection Molding, Pebble Gray
Dryflex® thermoplastic elastomers combine the performance of most vulcanized rubber with the process properties of thermoplastics. Dryflex® compounds permit sophisticated component design and thu..
Tensile Strength at Break 3.70 MPa
537 psi
ASTM D-412
Dynasol Solprene® 4318 Thermoplastic Rubber SBS Dry
Solprene 4318 is a linear block copolymer of styrene and butadiene, having 32% of styrene content, most of it forming a polystyrene block, which gives the polymer a thermoplastic behavior. It has a ..
Tensile Strength at Break 3.70 MPa
537 psi
ISO 527-1
Barlog Plastics KEBAFLEX E 45.1 TPE-V, Shore A45
TPE-VInformation provided by BARLOG plastics GmbH.