Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 3.45 MPa @Temperature 23.0 °C |
500 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versaflex™ OM 3060-1 Thermoplastic Elastomer (TPE) Versaflex™ OM 3060-1 is a clear, medical compliant overmold designed to adhere to multiple substrates. - Excellent bond to PC, ABS, PC/ABS, PC/PETG, and PC/PBT - Rubber Feel - Soft TouchVersaflex™.. |
|||
Tensile Strength at Break | 3.45 MPa | 500 psi | ASTM D638 |
Niche Polymer PA6GF13N Nylon 6, 13% Glass Fiber Filled Information provided by Niche Polymer |
|||
Tensile Strength at Break | 3.45 MPa | 500 psi | ASTM D412 |
Teknor Apex Monprene® MP 1869 Thermoplastic Elastomer Features: Monprene® TPE gels are softer than the shore A range of hardness. Monprene® TPE gels are high strength and high flow elastomers that may be used in the overmolding processes on poly.. |
|||
Tensile Strength at Break | 3.45 MPa | 500 psi | ASTM D412 |
Teknor Apex Monprene® MP-1736S Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 3.45 MPa | 500 psi | ASTM D412 |
Teknor Apex Monprene® MP-1829-R Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 3.45 MPa | 500 psi | ASTM D412 |
Teknor Apex Monprene® MP-2235 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 3.45 MPa | 500 psi | ASTM D412 |
Teknor Apex Monprene® MP-2260 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 3.45 MPa | 500 psi | ASTM D412 |
Teknor Apex Monprene® MP-2260-R1 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 3.45 MPa | 500 psi | ASTM D412 |
Teknor Apex Monprene® MP-2287 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 3.45 MPa | 500 psi | ASTM D412 |
Teknor Apex Monprene® MP-2315C Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 3.45 MPa | 500 psi | ASTM D412 |
Teknor Apex Monprene® MP 1128 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 3.45 - 4.14 MPa | 500 - 600 psi | |
Master Bond MasterSil 710 Silicone Paste Meets MIL Spec Description: MasterSil 710 is an easy to use, one component, high performance silicone elastomer compound for bonding, sealing, coating and formed in place gaskets. This product meets the Meets MIL-.. |
|||
Tensile Strength at Break | 3.45 MPa | 500 psi | ASTM D412 |
Teknor Apex Telcar® TL-3954-45 Thermoplastic Elastomer Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Insulation; Terminal Cable Jacketing; Underground Power Cable; Wire .. |
|||
Tensile Strength at Break | 3.45 MPa | 500 psi | |
Master Bond EP21TPFL-1AO Two Part, Flexible, Lower Viscosity Epoxy Polysulfide System Product Description: Master Bond EP21TPFL-1AO is a two component, low viscosity epoxy polysulfide for high performance bonding, sealing, coating and casting offering thermal conductivity, electrical.. |
|||
Tensile Strength at Break | 3.45 - 41.4 MPa | 500 - 6000 psi | |
Abatron BronzeWeld-PH™ Bronze-Filled, Structural Adhesive Putty; High Temperature Paste BronzeWeld-PH™ is BronzeWeld-P™ for up to 320° F (160° C) under stress. Used when it must resist up to 320° F in operation. Superior resistance to strong solvents and other chemicals. Technical.. |
|||
Tensile Strength at Break | 3.45 - 41.4 MPa | 500 - 6000 psi | |
Abatron Ferrobond-LH™ Steel-Filled, Structural Adhesive Putty; High Temperature Liquid Ferrobond-LH™ is Ferrobond-L™ for up to 320° F (160° C) under stress; Superior resistance to strong solvents and other chemicals. Technical Characteristics: A: 23 lbs/gal; B: 9.8 lbs/gal; mixin.. |
|||
Tensile Strength at Break | 3.45 - 41.4 MPa | 500 - 6000 psi | |
Abatron Ferrobond-PH™ Steel-Filled, Structural Adhesive Putty; High Temperature Paste Ferrobond-PH™ is Ferrobond-P™ for up to 320° F (160° C) under stress. Superior resistance to strong solvents and other chemicals. For resistance up to 160° C in operation. Technical Characteris.. |
|||
Tensile Strength at Break | 3.45 - 41.4 MPa | 500 - 6000 psi | |
Abatron Metalfix-PH™ Aluminum-Filled, Structural Adhesive Putty; High Temperature Paste Metalfix-PH™ is MetalFix-P™ for up to 320° F (160° C) under stress. Used when it must resist up to 320° F in operation. Superior resistance to strong solvents and other chemicals. Technical Cha.. |
|||
Tensile Strength at Break | 3.45 - 41.4 MPa | 500 - 6000 psi | |
Abatron Metalfix-P™ Aluminum-Filled, Structural Adhesive Putty; Paste Metalfix-P™ is an aluminum-filled, structural adhesive putty. Patch, bond, resurface metal, structural components, patterns, molds, pipes, tanks, sculptures, and appliances. Forms a permanent bond .. |
|||
Tensile Strength at Break | 3.45 - 41.4 MPa | 500 - 6000 psi | |
Abatron SS-Bond-P™ Stainless-Steel-Filled, Structural Adhesive Putty; Paste SS-Bond-P™ is a stainless-steel-filled structural adhesive putty. Used where a filler is needed that is as heavy, hard, and wear resistant as iron, but rustproof and more chemical resistant. Common.. |
|||
Tensile Strength at Break | 3.45 - 41.4 MPa | 500 - 6000 psi | |
Abatron BronzeWeld-P™ Bronze-Filled, Structural Adhesive Putty; Paste BronzeWeld-P™ is a bronze-filled structural adhesive putty. Ideal for statuary, antiques, boats, transportation equipment, vases, railings, metal furniture, metal trim, frames, and instruments. Use.. |
|||
Tensile Strength at Break | 3.45 - 41.4 MPa | 500 - 6000 psi | |
Abatron Metalfix-LH™ Aluminum-Filled, Structural Adhesive Putty; High Temperature Liquid Metalfix-LH™ is MetalFix-L™ for up to 320° F (160° C) under stress. Superior resistance to strong solvents and other chemicals. Technical Characteristics: A: 14.8 lbs/gal; B: 9.8 lbs/gal; mixin.. |
|||
Tensile Strength at Break | 3.45 - 41.4 MPa | 500 - 6000 psi | |
Abatron SS-Bond-PH™ Stainless-Steel-Filled, Structural Adhesive Putty; High Temperature Paste SS-Bond-PH™ is SS-Bond-P™ for up to 320° F (160° C) under stress. Superior resistance to strong solvents and other chemicals. Technical Characteristics: A: 26 lbs/gal; B: 9.8 lbs/gal; mixing ra.. |
|||
Tensile Strength at Break | 3.45 MPa | 500 psi | ASTM D412 |
Parker Chomerics CHO-MUTE 9005 Microwave Absorber Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 500 MHz to 18 GHz. CHO-MUTE 9005 incorporates a high tech silicon.. |
|||
Tensile Strength at Break | 3.45 MPa | 500 psi | Elastic; ASTM D412 |
Multibase Multi-Flex® A 6221 CUV A VY Dk Pewter TPO Thermoplastic Polyolefin Elastomer Forms: PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |