Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 3.26 MPa | 473 psi | |
Mallard Creek Polymers Rovene® 6118 Styrene-Acrylic Emulsion Applications: Rovene® 6118 is a silanated styrene-acrylic emulsion specifically designed for formulation of concrete sealers and performance coatings. It provides excellent adhesion to concrete a.. |