Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 3.17 MPa @Time 7200 sec |
460 psi @Time 2.00 hour |
Die C; ASTM D414 |
STAR Thermoplastic Alloys & Rubbers StarFlex® P 7335-1000 TPE Product Description: StarFlex P 7335-1000 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelExcellent ColorabilityGood WeatherabilityFDA and medical grades avai.. |
|||
Tensile Strength at Break | 3.17 MPa | 460 psi | (20 in/min), Molded Properties; ASTM D638 |
ExxonMobil Escorene™ UL 53019CC Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 53019CC is a copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Free Flowing Agent.. |