Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 26.00 MPa | 3770 psi | JIS-K-6723 |
Denka VINYKON W5230 PVC, W grade for non-migratory sheath and special items A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |