Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 25.4 MPa | 3680 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Packaging XPL319 Polyvinyl Chloride, Rigid (PVC, Rigid) NOTE: All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of.. |
|||
Tensile Strength at Break | 25.4 MPa | 3690 psi | ASTM D638 |
LyondellBasell Alathon® ETP H5057 High Density Polyethylene ApplicationsALATHON H 5057 is a multi-purpose high-flow resin that exhibits enhanced low temperature impact performance, enhanced processability and thermal stability for fast cycling in multi-cavit.. |
|||
Tensile Strength at Break | 25.4 MPa | 3680 psi | ASTM D638 |
ITW Devcon Metal Repair Aluminum Putty (F), Aluminum Information provided by ITW Devcon |