Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 25.376 MPa @Temperature 100 °C, Time 252000 sec |
3680.5 psi @Temperature 212 °F, Time 70.0 hour |
After Dry Heat Aging; ASTM D865 |
Seals Eastern 7168 Nitrile Rubber Nitrile for oil & gas serviceInformation provided by Seals Eastern, Inc. |