Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 21.7 MPa | 3150 psi | 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible 1351 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 21.7 MPa | 3150 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible 90067 Polyvinyl Chloride, Flexible (PVC, Flexible) Automotive OEM approval(s).Information provided by PolyOne |
|||
Tensile Strength at Break | 21.7 MPa | 3150 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible XV3860 Polyvinyl Chloride, Flexible (PVC, Flexible) All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high .. |
|||
Tensile Strength at Break | 21.7 MPa | 3150 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible R267AM Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 21.7 MPa | 3150 psi | ASTM D638 |
Teknor Apex APEX® 3601-85 Polyvinyl Chloride, Flexible Uses: Medical/Healthcare Applications Agency Ratings: NSF 61 Forms: Pellets Additional Information: Second Generation SeriesInformation Provided by Teknor Apex |
|||
Tensile Strength at Break | 21.7 MPa | 3150 psi | ASTM D638 |
Teknor Apex APEX® 01-A0303E-95 Polyvinyl Chloride, Flexible Notes: 105°C Insulation; RoHS Compliant Uses: Automotive Electronics; Insulation; Wire and Cable Applications Wire Types: GPT Agency Ratings: SAE J1128 Forms: PelletsInformation Provided by Tekno.. |
|||
Tensile Strength at Break | 21.7 MPa | 3150 psi | ASTM D638 |
Plastics Group Polifil® RMC-40V 40% Calcium Carbonate-Reinforced Polypropylene, High Impact, UV Stabilized Polifil® RMC-V series compounds are high impact, UV stabilized polypropylenes reinforced with fine particle size calcium carbonate. In addition to the highest impact possible, these compounds retar.. |
|||
Tensile Strength at Break | 21.7 MPa | 3150 psi | ASTM D3759 |
3M 3380 HVAC Construction General purpose aluminum foil tape. Go to product for this market. UL 723 Classified.Information provided by 3M |