Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 20.1 MPa @Temperature 200 °C, Time 252000 sec |
2910 psi @Temperature 392 °F, Time 70.0 hour |
After Dry Heat Aging; ASTM D865 |
Seals Eastern 7182D Fluorocarbon-Elastomer Formulated AFLAS® high-temperature "sour" oil & gas service. Excellent acid and base resistance.Information provided by Seals Eastern, Inc. |
|||
Tensile Strength at Break | 20.1 MPa | 2910 psi | ASTM D412 |
Teknor Apex APEX® 3090-H Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Good FlexibilityUses-General Purpose, ProfilesAppearance-Natural Color, OpaqueForms-PelletsProcessin.. |
|||
Tensile Strength at Break | 20.1 MPa | 2920 psi | ASTM D1414, ASTM D412 |
DuPont Performance Polymers Kalrez® AeroSeal™ 7800 Fluoroelastomer Kalrez AeroSeal™ 7800* perfluoroelastomer parts are a specialty black product that meets the requirements of Aerospace Material Specification (AMS) 7257. It offers outstanding thermal stability and.. |
|||
Tensile Strength at Break | 20.1 MPa | 2920 psi | |
Asahi Glass Fluon® PB3060 60% Bronze, PTFE Filled Compound Fluon®PTFE FC has improved creep and wear resistance. A wide range of fillers such as glass fiber, graphite, bronze, carbon fiber are available. Information provided by Asahi Glass Company, Inc. |