Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 2.30 MPa @Time 7200 sec |
333 psi @Time 2.00 hour |
Die C; ASTM D414 |
STAR Thermoplastic Alloys & Rubbers StarMediflex P 7026-1000 TPE Product Description: StarMediflex P 7026-1000 is an easy processing TPE designed for injection molding. This particular class of TPE material for medical products and tubing applications. Features:S.. |
|||
Tensile Strength at Break | 2.30 MPa | 334 psi | |
3M 3635-91 Diffuser Film Control light transmission or achieve special effects for backlit signs; 2 and 4-mil vinyl film; Pressure-sensitive adhesive and Adheres to rigid or flexible substratesInformation provided by 3M |
|||
Tensile Strength at Break | 2.30 MPa | 334 psi | |
3M 3635-0171 Diffuser Film Control light transmission or achieve special effects for backlit signs; 2 and 4-mil vinyl film; Pressure-sensitive adhesive and Adheres to rigid or flexible substratesInformation provided by 3M |
|||
Tensile Strength at Break | 2.30 MPa | 334 psi | ISO 527-1 |
Barlog Plastics KEBAFLEX SG 25 A.1 TPE-S, Shore A25, natural TPE-SInformation provided by BARLOG plastics GmbH. |
|||
Tensile Strength at Break | 2.30 MPa | 334 psi | |
3M 3635-20b Diffuser Film Control light transmission or achieve special effects for backlit signs; 2 and 4-mil vinyl film; Pressure-sensitive adhesive and Adheres to rigid or flexible substratesInformation provided by 3M |
|||
Tensile Strength at Break | 2.30 MPa | 334 psi | |
3M 3635-22b Diffuser Film Control light transmission or achieve special effects for backlit signs; 2 and 4-mil vinyl film; Pressure-sensitive adhesive and Adheres to rigid or flexible substratesInformation provided by 3M |