Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 19.9 MPa | 2890 psi | Across Flow; ASTM D412 |
ExxonMobil Vyram™ 9103-45 Thermoplastic Elastomer
(discontinued **) A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi.. |
|||
Tensile Strength at Break | 19.9 MPa | 2890 psi | Across Flow; ASTM D412 |
ExxonMobil Vyram™ 9203-45 Thermoplastic Elastomer
(discontinued **) A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character.. |
|||
Tensile Strength at Break | 19.9 MPa | 2880 psi | ASTM D412 |
Teknor Apex MF 141 Polyvinyl Chloride, Flexible Film Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Film, Medical Applications Forms-PelletsAppearance-ClearInformation provided by Teknor Apex Company |
|||
Tensile Strength at Break | 19.9 MPa | 2880 psi | ASTM D3759 |
3M Scotch® 8915 Filament Tape Scotch® Filament Tape 8915 is a high-performance transparent tape reinforced with continuous high strength glass filaments which is designed to hold appliance parts together during manufacture and .. |
|||
Tensile Strength at Break | 19.9 MPa | 2880 psi | ASTM D3759 |
3M Scotch® 8916 Filament Tape Scotch® Filament Tape 8916 is a high-performance transparent tape reinforced with continuous high strength glass filaments which is designed to hold appliance parts together during manufacture and .. |
|||
Tensile Strength at Break | 19.9 MPa | 2880 psi | ASTM D3759 |
3M Scotch® 897 Filament Tape Scotch® Tape 897 is a glass-filament-reinforced tape suitable for light to medium duty strapping, bundling, reinforced applications. Scotch® Tape 897 has a synthetic rubber resin adhesive with goo.. |