Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 19.7 MPa | 2860 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible R340AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 19.7 MPa | 2860 psi | 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible B5D01 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 19.7 MPa | 2860 psi | ISO 527 |
LG Chemical LUTENE XL8080NT PE Compound Description: LUTENE XL8080NT is a standard version having excellent electrical properties for medium and high voltage power cable insulation and has a very low level of contamination.Applications: M.. |
|||
Tensile Strength at Break | >= 19.7 MPa | >= 2860 psi | ISO 527 |
LG Chemical LUTENE XL8080UC PE Compound Description: LUTENE XL8080UC is a superior cleanliness version for high voltage power cable insulation and is designated as UC (Ultra-Clean) due to its extremely low level of contamination. LUTENE X.. |
|||
Tensile Strength at Break | 19.7 MPa | 2850 psi | ASTM D638 |
Teknor Apex APEX® 3601-80 Polyvinyl Chloride, Flexible Uses: Medical/Healthcare Applications Agency Ratings: NSF 61 Forms: Pellets Additional Information: Second Generation SeriesInformation Provided by Teknor Apex |
|||
Tensile Strength at Break | 19.7 MPa | 2850 psi | ASTM D638 |
Teknor Apex APEX® 82-E211-B Polyvinyl Chloride, Flexible Notes: 80°C Insulation; RoHS Compliant Uses: Transportation Wire Insulation Agency Ratings: SAE J1128 Automotive Specifications: Chrysler MS-DC16 Type A Processing Method: Extrusion Forms: Pell.. |
|||
Tensile Strength at Break | 19.7 MPa | 2850 psi | ASTM D638 |
Teknor Apex APEX® 84468 Polyvinyl Chloride, Flexible Notes: 105°C Jacket; RoHS Compliant Features: Flame Retardant; Good UV Resistance Uses: Cable Jacketing; Insulation Forms: Pellets Agency Ratings: UL 1063; UL 1581; UL 62Information Provided by T.. |
|||
Tensile Strength at Break | 19.7 MPa | 2860 psi | ASTM D638 |
Teknor Apex APEX® 96-A0914K-106 Polyvinyl Chloride, Flexible Notes: 105°C Jacket; RoHS Compliant Uses: Wire and Cable ApplicationsForms: PelletsInformation Provided by Teknor Apex |
|||
Tensile Strength at Break | 19.7 MPa | 2850 psi | ASTM C307 |
Chesterton ARC 791 Composite Description: A quartz reinforced composite designed to resurface and restore concrete surfaces, to protect new concrete, and to repair concrete damaged by chemical and physical abuse. ARC 791 has ex.. |
|||
Tensile Strength at Break | 19.7 MPa | 2850 psi | ASTM D412 |
Compuestos Dominicanos Polycom AM-05495 PVC Compound The polycom AM series are designed for the covering of wires for the production of fences. They are available in different colors and all provide excellent UV light and microorganisms resistance. A.. |
|||
Tensile Strength at Break | 19.7 MPa | 2850 psi | ASTM D412 |
Compuestos Dominicanos Polycom AM-050495 PVC Description: The polycom AM series compounds are designed for the covering of wires for the production of fences. These products are available in different colors and have excellent properties of U.. |
|||
Tensile Strength at Break | 19.7 MPa | 2850 psi | ASTM D412 |
Compuestos Dominicanos Polycom AM-440495 PVC Compound The polycom AM series are designed for the covering of wires for the production of fences. They are available in different colors and all provide excellent UV light and microorganisms resistance. A.. |
|||
Tensile Strength at Break | 19.7 MPa | 2850 psi | ASTM D412 |
Compuestos Dominicanos Polycom AU-050695 PVC Compound Compuestos Dominicanos, S.A. manufactures high quality covering PVC for the production of electrical wire and cable providing excellent insulation properties and smooth finish. Their products are d.. |