Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 18.6 MPa | 2700 psi | 2 in/min; ASTM D638 |
RheTech Products FT4900-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | 2 in/min; ASTM D638 |
RheTech Products FT4900-33UV Thermoplastic Polyolefin, UV Stabilized, KSD Charcoal Argent Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | 2 in/min; ASTM D638 |
RheTech Products FT4900-745UV Thermoplastic Polyolefin, UV Stabilized, CJM Medium Khaki Solid Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | 2 in/min; ASTM D638 |
RheTech Products FT4900-772UV Thermoplastic Polyolefin, UV Stabilized, RXF Jet Black Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ HC 2180 Polyvinyl Chloride, Flexible (PVC, Flexible) Geon HC 2180 is a 80 Shore A non-phthalate flexible vinyl compound made from FDA sanctioned ingredients. HC 2180 can be used for extrusion and injection molding healthcare applications.NOTE: All ing.. |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible A90U2 Polyvinyl Chloride, Flexible (PVC, Flexible) GENERAL PURPOSE CLEAR PVC COMPOUND WITH LOW LEVEL OF U.V. INHIBITOR, to be used only in interior applications.Information provided by PolyOne |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible G92D Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible R1700D Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible R235AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible XV 3432 Trans 9000 Polyvinyl Chloride, Flexible (PVC, Flexible) This product has received full compliance certification for USP Biological Reactivity Tests under USP Plastic Class VI.NOTE: All ingredients used in the formulation of this compound are listed in th.. |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible XV3856 Polyvinyl Chloride, Flexible (PVC, Flexible) All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high .. |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible R235AE White 1875 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible R356AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible R363MB White 1876 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | ASTM D4894 |
3M Dyneon™ CCX6380 PTFE, 10% Polyimide Filler
(discontinued **) Type II, free flowing.Typical Applications: Finished or semi-finished parts: sheets, rods, tubes, billets for skiving of films or machining into complex shapes.Information provided by the Dyneon div.. |
|||
Tensile Strength at Break | 18.6 - 20.7 MPa | 2700 - 3000 psi | |
ITW Plexus Plexusâ„¢ AO420 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose adhesive , high toughness.Information provided by Illinois Tool Works. |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | 2 in/min; ASTM D638 |
Ineos R05C-00 Polypropylene Random Copolymer Random copolymer R05C-00 is an antistatic, clarified polypropylene random copolymer produced by a unique catalyst technology. It is designed as a high gloss resin and exhibits good stiffness and imp.. |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | ASTM D638 |
Teknor Apex APEX® 3710-85NT1 Polyvinyl Chloride, Flexible Notes: RoHS Compliant Uses: Medical/Healthcare Applications Forms: PelletsInformation Provided by Teknor Apex |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | ASTM D638 |
Teknor Apex APEX® 4107 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | ASTM D638 |
Teknor Apex APEX® 84459 Polyvinyl Chloride, Flexible Notes: 105°C Insulation; RoHS Compliant Features: Flame Retardant; Low to no Migration; Oil ResistantUses: Insulation Agency Ratings: UL 1063; UL 62; UL 1581 Forms: Pellets Wire Types: AWMInforma.. |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | ASTM D638 |
Teknor Apex MF 165-J3 NT Polyvinyl Chloride, Flexible Film Uses: Medical/Healthcare Applications Forms: FilmInformation Provided by Teknor Apex |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | ASTM D638 |
Teknor Apex Synres® SR 4336 Polypropylene Notes: The Specialty Compounding Division offers a proprietary line of mineral filled polyolefins, including talc and calcium carbonate filled polypropylenes. Typical applications include injection .. |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | ASTM D412 |
Teknor Apex Telcar® TL-101 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | ASTM D412 |
UBE UBEPOL VCR406 Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C) Description: UBEPOL-VCR is a new type of synthetic rubber system developed by UBE's original technology. UBEPOL-VCR consists of micro-dispersed syndiotactic 1,2-polybutadiene (SPB) with high mel.. |
|||
Tensile Strength at Break | 18.6 MPa | 2690 psi | ASTM D3759 |
3M Scotch Pad™ 819 Filament Tape Pads 3M™ ScotchPad™ Filament Tape Pad 819 is a pre-cut pad formed with layered high performance filament tape sheets featuring biaxially oriented polypropylene backing with continuous glass yarns that .. |
|||
Tensile Strength at Break | 18.6 MPa | 2700 psi | ASTM D1708 |
DuPont Elvax® 4260 Ethylene Vinyl Acetate
(discontinued **) DuPont™ Elvax® 4260 is an ethylene-vinyl acetate / acid terpolymer resin for use in industrial applications. Applications:Elvax® 4260 resins can be used for the following applications: adhesives,.. |