Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 18.4 MPa | 2670 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible R291AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 18.4 MPa | 2670 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible XV3844 Polyvinyl Chloride, Flexible (PVC, Flexible) All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high .. |
|||
Tensile Strength at Break | 18.4 MPa | 2670 psi | ASTM D412 |
UBE UBEPOL VCR406 Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C) Description: UBEPOL-VCR is a new type of synthetic rubber system developed by UBE's original technology. UBEPOL-VCR consists of micro-dispersed syndiotactic 1,2-polybutadiene (SPB) with high mel.. |
|||
Tensile Strength at Break | 18.4 MPa | 2670 psi | Air at 302°F, 168 hr; ASTM D573 |
ExxonMobil Santoprene® 103-40 Thermoplastic Elastomer A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Tensile Strength at Break | >= 18.4 MPa | >= 2670 psi | |
3M Scotchcal™ 50-1 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Tensile Strength at Break | >= 18.4 MPa | >= 2670 psi | |
3M Scotchcal™ 50-10 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Tensile Strength at Break | >= 18.4 MPa | >= 2670 psi | |
3M Scotchcal™ 50-12 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Tensile Strength at Break | >= 18.4 MPa | >= 2670 psi | |
3M Scotchcal™ 50--120 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Tensile Strength at Break | >= 18.4 MPa | >= 2670 psi | |
3M Scotchcal™ 50-24 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Tensile Strength at Break | >= 18.4 MPa | >= 2670 psi | |
3M Scotchcal™ 50-27 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Tensile Strength at Break | >= 18.4 MPa | >= 2670 psi | |
3M Scotchcal™ 50-44 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Tensile Strength at Break | >= 18.4 MPa | >= 2670 psi | |
3M Scotchcal™ 50-483 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Tensile Strength at Break | >= 18.4 MPa | >= 2670 psi | |
3M Scotchcal™ 50-49 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Tensile Strength at Break | >= 18.4 MPa | >= 2670 psi | |
3M Scotchcal™ 50-64 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Tensile Strength at Break | >= 18.4 MPa | >= 2670 psi | |
3M Scotchcal™ 50-66 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Tensile Strength at Break | >= 18.4 MPa | >= 2670 psi | |
3M Scotchcal™ 50-745 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Tensile Strength at Break | >= 18.4 MPa | >= 2670 psi | |
3M Scotchcal™ 50-76 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Tensile Strength at Break | >= 18.4 MPa | >= 2670 psi | |
3M Scotchcal™ 50-79 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Tensile Strength at Break | >= 18.4 MPa | >= 2670 psi | |
3M Scotchcal™ 50-88 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Tensile Strength at Break | >= 18.4 MPa | >= 2670 psi | |
3M Scotchcal™ 50-90 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Tensile Strength at Break | >= 18.4 MPa | >= 2670 psi | |
3M Scotchcal™ 50-914 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Tensile Strength at Break | >= 18.4 MPa | >= 2670 psi | |
3M Scotchcal™ 50-97 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Tensile Strength at Break | 18.4 MPa | 2670 psi | ASTM D3759 |
3M 695 Riveters Tape 3M™ Riveters Tape 695 is a zone-coated polyethylene film tape with a tack-free center “window” for use in holding aircraft rivets in place prior to and during riveting.Information provided by 3M |
|||
Tensile Strength at Break | >= 18.4 MPa | >= 2670 psi | |
3M Scotchcal™ 50-100 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Tensile Strength at Break | >= 18.4 MPa | >= 2670 psi | |
3M Scotchcal™ 50-34 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Tensile Strength at Break | >= 18.4 MPa | >= 2670 psi | |
3M Scotchcal™ 50-58 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Tensile Strength at Break | >= 18.4 MPa | >= 2670 psi | |
3M Scotchcal™ 50-78 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Tensile Strength at Break | >= 18.4 MPa | >= 2670 psi | |
3M Scotchcal™ 50-82 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Tensile Strength at Break | >= 18.4 MPa | >= 2670 psi | |
3M Scotchcal™ 50-92 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |