Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 15.7 MPa | 2280 psi | ISO 37 |
PolyOne OnFlex™ V 3040D-S0093 Thermoplastic Elastomer (TPE) OnFlex™-V provides the performance of traditional vulcanised rubber, but with the processability of a thermoplastic. OnFlex™-V 3000 series thermoplastic elastomer compounds are based on a polyolef.. |
|||
Tensile Strength at Break | 15.7 MPa | 2280 psi | |
NEU NeuSoft™ 597-60A Industrial Ether TPU / SBC blend |
|||
Tensile Strength at Break | 15.7 MPa | 2280 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible R111AE Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength at Break | 15.7 MPa | 2280 psi | 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible 90057 Polyvinyl Chloride, Flexible (PVC, Flexible) Automotive OEM approval(s).Information provided by PolyOne |
|||
Tensile Strength at Break | 15.7 MPa | 2280 psi | After 70hrs @347°F in Stauffer 7700 |
Greene Tweed FLUORAZ® 799 Fluoroelastomer, FEPM Greene, Tweed`s Fluoraz® functions effortlessly in a variety of challenging process environments. Fluoraz performs well in aggressive chemicals where ultrapure materials are not required. Known f.. |
|||
Tensile Strength at Break | 15.7 MPa | 2280 psi | ISO R 527 |
Stir SpA SR 88 (PVC) Application: Primary type R 2Information provided by STIR SpA |
|||
Tensile Strength at Break | 15.7 MPa | 2280 psi | ASTM D638 |
3M Scotchkote™ HB 850 Epoxy Floor Coating Scotchkote Epoxy Floor Coating HB 850 has been specifically developed as a 100% solids protection system for application to a wide rage of floor surfaces.Product Features:Combines good application c.. |
|||
Tensile Strength at Break | 15.7 MPa | 2280 psi | ASTM D638 |
Teknor Apex APEX® 82-E378-H Polyvinyl Chloride, Flexible Notes: RoHS Compliant Features: Flame Retardant Uses: Cable Jacketing Agency Ratings: UL 62 Wire Types: SJT; ST; VW-1 Forms: PelletsInformation Provided by Teknor Apex |
|||
Tensile Strength at Break | 15.7 MPa | 2280 psi | 5mm/min; ASTM D638 |
Mitsui TPX® MX002 Methylpentene Copolymer TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi.. |