Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 138 MPa | 20000 psi | ASTM D638 |
Polymer Resources TP-HG40 Polybutylene Terephthalate, 40% Glass Reinforced Alloy Polybutylene Terephthalate, 40% Glass Reinforced AlloyProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informatio.. |
|||
Tensile Strength at Break | 138 MPa | 20000 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Edgetek® PC-15CF-15GF/000 Polycarbonate (PC) Information provided by PolyOne |
|||
Tensile Strength at Break | 138 MPa | 20000 psi | Type I, 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Lubricomp PFL34 PA 6 LNP* Lubricomp* PFL34 is a compound based on Nylon 6 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Am.. |
|||
Tensile Strength at Break | 138 MPa | 20000 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Lubricomp PFL34 PA 6 LNP* Lubricomp* PFL34 is a compound based on Nylon 6 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Am.. |
|||
Tensile Strength at Break | 138 MPa | 20000 psi | ASTM D638 |
Techmer ES Plaslube® J-4/30/TF/13/SI/2 NAT PA6/12 |
|||
Tensile Strength at Break | 138 MPa @Temperature 23.0 °C |
20000 psi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® PLUS PLSFR95G15DH2 BK269 Nylon
(Unverified Data**) Zytel® PLSFR95G15DH2 BK269 is 15% glass reinforced, flame retardant black PA using SHIELD Technology, only from DuPont, exceptional resistance in hot air & hot engine oil.Information provided by Du.. |
|||
Tensile Strength at Break | 138 MPa | 20000 psi | 5 mm/min; ISO 527 |
Eurostar Staramide BG6ST01 PA6, Glass Fiber Filled, Impact Modified, Injection Molded Staramide BG6ST01 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |