Mechanical Properties Metric English Comments
Tensile Strength at Break 11.1 MPa
1610 psi
510 mm/min; ASTM D412A
PolyOne Elastamax™ XL-2165 Thermoplastic Polyolefin Elastomer (TPO (POE))
PolyOne's Elastamax™ XL thermoplastic olefins (TPOs) are based on pelletized blends of polyolefin resins and select elastomers such EPDM. These materials have been engineered to provide a balance o..
Tensile Strength at Break 11.1 MPa
1610 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 241-80 Thermoplastic Elastomer  (discontinued **)
A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and NSF 51 f..
Tensile Strength at Break >= 11.1 MPa
>= 1610 psi
after aging (168h, 150°C); ASTM D412
Borealis PC0798 Polyethylene Insulation Compound, Crosslinkable
PC0798 is a flame retardant crosslinking polyethylene compound for low voltage insulation. PC0798 is a halogenated, colorable, chemically crosslinkable copolymer compound which contains flame retar..
Tensile Strength at Break 11.1 MPa
1610 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 201-80 Thermoplastic Elastomer
A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra..
Tensile Strength at Break 11.1 MPa
1610 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 271-80 Thermoplastic Elastomer
A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t..
Tensile Strength at Break 11.1 MPa
1610 psi
ISO 37
Alliance Polymers Viprene™ G85A-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G85A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Strength at Break 11.1 MPa
1610 psi
ASTM D412
Advanced Polymer Alloys Alcryn® 2160 BK Melt Processable Rubber
Alcryn 2100 Series melt-processable rubber (MPR) offer a broader range of bonding to rigid substrates while maintaining all the excellent performance features of traditional Alcryn. The 2100 grades..
Tensile Strength at Break 11.1 MPa
1610 psi
ISO 37
Alliance Polymers Viprene™ G85A-32U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G85A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Strength at Break 11.1 MPa
1610 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 101-80 Thermoplastic Elastomer
A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range ..
Copyright © lookpolymers.com All Rights Reserved