Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 10.7 MPa | 1550 psi | 510 mm/min; ASTM D412A |
PolyOne Synprene™ RT-5180 RoHS Natural Styrene Butadiene Block Copolymer (SBC) Synprene™ thermoplastic elastomers (TPEs) are compounds based on styrenic block copolymer (SBC) technology, and can be formulated to deliver extremely low hardness values not found in other elastom.. |
|||
Tensile Strength at Break | 10.7 MPa @Temperature 23.0 °C |
1550 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versaflex™ CL E85 Thermoplastic Elastomer (TPE) Versaflex™ CL E85 is an exceptional clarity, high performance and autoclavable solution ideal for healthcare and food packaging. Versaflex™ CL E85 is also formulated without the use of plasticizer.. |
|||
Tensile Strength at Break | 10.7 MPa @Temperature 23.0 °C |
1550 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7990-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7990-1001-00 is an easy processing, general purpose TPE designed for a wide variety of applications. - Overmold Adhesion to Polypropylene - Rubbery FeelDynaflex™ G7990-1001-00 can be re.. |
|||
Tensile Strength at Break | 10.7 MPa @Temperature 23.0 °C |
1550 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7990-9001-02 Thermoplastic Elastomer (TPE) Dynaflex™ G7990-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications. - Overmold Adhesion to Polypropylene - Rubbery FeelDynaflex™ G7990-9001-02 can be re.. |
|||
Tensile Strength at Break | 10.7 MPa | 1550 psi | Type IV, 510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible XV3855 Polyvinyl Chloride, Flexible (PVC, Flexible) XV3855 is a flexible (57A durometer) vinyl compound formulated from FDA-santioned raw materials. XV3855 Clear 1869 has been tested to USP Class VI.NOTE: All ingredients used in the formulation of th.. |
|||
Tensile Strength at Break | 10.7 MPa | 1550 psi | IEC 60811 |
Solvay Specialty Polymers Cogegum® AFR/930 Polyolefin, Unspecified
(discontinued **) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
Tensile Strength at Break | 10.7 MPa | 1550 psi | ASTM D1414 |
Greene Tweed CHEMRAZ® 571 Perfluoroelastomer Chemraz® 571 is recommended for a wide variety of semiconductor equipment wet processing applications where stringent seal reliability and contamination control are required. This seal material .. |
|||
Tensile Strength at Break | 10.7 MPa | 1550 psi | |
Shin-Etsu Silicones KEP-12 Silicone additive KEP12 is an additive which can be used in most of the silicone products to improve heat stability.Product Features: Improve thermal stability and compression set.Excellent dispersion.Information Pro.. |
|||
Tensile Strength at Break | 10.7 MPa | 1550 psi | ASTM D412 |
Teknor Apex APEX® 2060-H Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Good FlexibilityUses-General Purpose, ProfilesAppearance-ClearForms-PelletsProcessing Method-Extrusi.. |
|||
Tensile Strength at Break | 10.7 MPa | 1550 psi | ASTM D638 |
Teknor Apex APEX® 76-5179-B Polyvinyl Chloride, Flexible Notes: 80°C General Purpose; RoHS Compliant Features: Flame Retardant Uses: Wire and Cable ApplicationsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709Addition.. |
|||
Tensile Strength at Break | 10.7 MPa | 1550 psi | ASTM D638 |
Teknor Apex APEX® 87-L417D-NT Polyvinyl Chloride, Flexible Notes: RoHS Compliant Forms: PelletsInformation Provided by Teknor Apex |
|||
Tensile Strength at Break | 10.7 MPa | 1550 psi | ASTM D638 |
Teknor Apex APEX® 90-A471R-60-NT Polyvinyl Chloride, Flexible Features: DEHP Plasticizer; Radiation (Gamma) Resistant; Radiation Sterilizable Uses: Medical/Healthcare Applications; Tubing Processing Method: Extrusion Forms: PelletsInformation Provided by Tekno.. |
|||
Tensile Strength at Break | 10.7 MPa | 1550 psi | ASTM D638 |
Teknor Apex HFFR 2003 Polyolefin, Halogen Free Notes: RoHS Compliant Features: Flame Retardant; Halogen Free Uses: Communication Wire Jacketing; Electronic Cable Jacketing; Security Cable Jacketing; Fiber Optic Cable Agency Ratings: IEC 60332-1;.. |
|||
Tensile Strength at Break | 10.7 MPa | 1550 psi | DBPH Cure |
Shin-Etsu Silicones KE-5551U High Strength Silicone Elastomer ShinEtsu KE5551 U is a nominal 50 Durometer base which offers high tensile and tear strengths. Its excellent processing characteristics make it suitable for molding, extrusion and calendaringProduct.. |
|||
Tensile Strength at Break | 10.7 MPa | 1550 psi | 20 in/min; ASTM D412 |
Teknor Apex Telcar® TL-1934E Styrenic Thermoplastic Elastomer Uses: Appliance Wire Insulation; Cable Jacketing; Flexible Cord Insulation; Wire and Cable Applications; Wire Jacketing Agency Ratings: UL 1581 Forms: Pellets Processing Method: Extrusion; Injection.. |
|||
Tensile Strength at Break | 10.7 MPa | 1550 psi | ASTM D638 |
Westlake Elevate™ EF526 16% Ethylene Vinyl Acetate Copolymer Westlake Elevate™ EF526 resin is a 16% EVA copolymer designed for cast film, extrusion coatings, and thermal laminations.Application/UsesThermal laminationsCast FilmExtrusion CoatingsThis resin gra.. |
|||
Tensile Strength at Break | 10.7 MPa | 1550 psi | ASTM D3759 |
3M Scotch® 356 Transparent Label Protection Tape Scotch® Label Protection Tape 356 is a transparent, tough film tape made especially for label protection in outdoor applications or where the application demands extra resistance to moisture, chemi.. |