Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 10.608 MPa | 1538.5 psi | Air at 302°F, 168 hr; ASTM D573 |
ExxonMobil Santoprene® 111-87 Thermoplastic Elastomer
(discontinued **) A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Tensile Strength at Break | 10.608 MPa | 1538.5 psi | Air at 302°F, 168 hr; ASTM D573 |
ExxonMobil Santoprene® 211-87 Thermoplastic Elastomer
(discontinued **) A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |