Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 10.38 MPa | 1505 psi | |
Shin-Etsu Silicones KE-5540U Low Temperature Silicone Elastomer ShinEtsu KE5540 U is a nominal 40 Durometer phenyl (PVMQ) base.Product Features: This material was designed for its excellent vibration dampening characteristics. Because of its phenyl content, it a.. |