Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 1.70 MPa | 247 psi | ASTM D3759 |
3M 2104 Polyethylene Protective Tapes 3M™ Polyethylene Protective Tapes 2104 has a very low-tack adhesive system to helpInformation provided by 3M |
|||
Tensile Strength at Break | 1.70 MPa | 247 psi | ASTM D3759 |
3M 2105 (Clear) Polyethylene Protective Tapes 3M™ Polyethylene Protective Tapes 2105 has a very low-tack adhesive system to helpInformation provided by 3M |
|||
Tensile Strength at Break | 1.70 MPa | 247 psi | ASTM D3759 |
3M 2110 Polyethylene Protective Tapes 3M™ Polyethylene Protective Tapes 2110 has a very low-tack adhesive system to help provide temporary protection of many polished metals, smooth plastics and glass materials with minimum adhesion bu.. |
|||
Tensile Strength at Break | 1.70 MPa | 247 psi | ASTM D3759 |
3M 2187 Polyethylene Protective Tapes 3M™ Polyethylene Protective Tapes 2187 has a high-tack adhesive system to help provide temporary protection of many metals, plastics and painted metal panels with minimum adhesion build up and clea.. |
|||
Tensile Strength at Break | 1.70 MPa | 247 psi | ASTM D3759 |
3M 3105 (Clear) Polyethylene Protective Tapes 3M™ Polyethylene Protective Tapes 3105 has a low-tack adhesive system to help provide temporary protection of many polished metals, smooth plastics, glass materials and high gloss painted surfaces... |
|||
Tensile Strength at Break | 1.70 MPa | 247 psi | ASTM D3759 |
3M 3125 (Clear) Polyethylene Protective Tapes 3M™ Polyethylene Protective Tapes 3125 has a low-tack adhesive system to help provide temporary protection of mill finished stainless and aluminum coils or sheets with minimum adhesion buildup and .. |
|||
Tensile Strength at Break | 1.70 MPa | 247 psi | ASTM D3759 |
3M 3126 Polyethylene Protective Tapes 3M™ Polyethylene Protective Tapes 3126 has a medium-tack adhesive system to help provide temporary protection of many finished metals, plastics and painted building panels with minimum adhesion bui.. |
|||
Tensile Strength at Break | 1.70 MPa | 247 psi | ASTM D3759 |
3M 3187 (Clear) Polyethylene Protective Tapes 3M™ Polyethylene Protective Tapes 3187 has a high-tack adhesive system to help provide temporary protection of many textured metals, plastics and molded fiberglass materials with minimum adhesion b.. |
|||
Tensile Strength at Break | 1.70 MPa | 247 psi | ASTM D3759 |
3M 4112 (Clear) Polyethylene Protective Tapes 3M™ Polyethylene Protective Tapes 4112 has a low-tack adhesive system to help provide temporary protection for many metals, plastics, vinyls and glass materials.Information provided by 3M |
|||
Tensile Strength at Break | 1.70 MPa | 247 psi | ASTM D3759 |
3M 4125 Polyethylene Protective Tapes 3M™ Polyethylene Protective Tapes 4125 has a low-tack adhesive system to help provide temporary protection for many metals, plastics and glass materials.Information provided by 3M |
|||
Tensile Strength at Break | 1.70 MPa | 247 psi | ASTM D3759 |
3M 4179 (Clear) Polyethylene Protective Tapes 3M™ Polyethylene Protective Tapes 4179 has a very high-tack adhesive system to help provide temporary protection of many dissimilar metals, automotive carpeting, carpeted door panels and plastic sc.. |
|||
Tensile Strength at Break | 1.70 MPa | 247 psi | ASTM D3759 |
3M 4187 (Clear) Polyethylene Protective Tapes 3M™ Polyethylene Protective Tapes 4187 has a high-tack adhesive system to help provide temporary protection to a variety of materials that have textured surfaces.Information provided by 3M |
|||
Tensile Strength at Break | 1.70 MPa | 247 psi | ASTM D3759 |
3M 4188 (Clear) Polyethylene Protective Tapes 3M™ Polyethylene Protective Tapes 4188 has a high-tack adhesive system to help provide temporary protection for many textured laminates, brushed metals and coarse plastic materials.Information prov.. |
|||
Tensile Strength at Break | 1.70 MPa | 247 psi | ASTM D412 |
3M 730 Clear Hybrid Sealant 3M™ 700-Series Hybrid Sealant and Hybrid Adhesive Sealant products are one component, moisture curing products which form permanent elastic bonds. They are similar in function as a typical one comp.. |
|||
Tensile Strength at Break | 1.70 MPa | 247 psi | ASTM D3759 |
3M Cold Seal® 3130 Polyethylene Tape 3M™ Cold Seal® Polyethylene Tape 3130 is a temporary tape with a self-sealing latex emulsion and feature a self-adhering cohesive coating which bonds to itself and not to the product to be package.. |
|||
Tensile Strength at Break | 1.70 MPa | 247 psi | ASTM D3759 |
3M 2125 Polyethylene Protective Tapes 3M™ Polyethylene Protective Tapes 2125 has a medium-tack adhesive system to help provide temporary protection of many metals, plastics and painted metal panels with minimum adhesion build up and cl.. |
|||
Tensile Strength at Break | 1.70 MPa | 247 psi | ASTM D3759 |
3M 2112 Polyethylene Protective Tapes 3M™ Polyethylene Protective Tapes 2112 has a very low-tack adhesive system to help provide temporary protection of many polished metals, smooth plastics and glass materials with minimum adhesion bu.. |
|||
Tensile Strength at Break | 1.70 MPa | 247 psi | ASTM D3759 |
3M 3179 (Clear) Polyethylene Protective Tapes 3M™ Polyethylene Protective Tapes 3179 has a very high tack adhesive system to help provide temporary protection of plastics and fabrics.Information provided by 3M |
|||
Tensile Strength at Break | 1.70 MPa | 247 psi | ASTM D3759 |
3M 3195-EZ Polyethylene Protective Tapes 3M™ Polyethylene Protective Tapes 3195-EZ is an easy unwind tapes coated with a very high-tack adhesive system to help provide temporary protection of automotive carpets, fabric interiors and carpe.. |
|||
Tensile Strength at Break | 1.70 MPa | 247 psi | ASTM D3759 |
3M 4126 (Clear) Polyethylene Protective Tapes 3M™ Polyethylene Protective Tapes 4126 has a low-tack adhesive system to help provide temporary protection for many metals, plastics and glass materials.Information provided by 3M |
|||
Tensile Strength at Break | 1.70 MPa | 247 psi | ASTM D3759 |
3M 4167 (Clear) Polyethylene Protective Tapes 3M™ Polyethylene Protective Tapes 4167 has a very high-tack adhesive system designed to help provide temporary protection of vinyl, and high-pressure matte laminates, textured plastics and can be a.. |
|||
Tensile Strength at Break | 1.70 MPa | 247 psi | ASTM D3759 |
3M 4193-EZ Polyethylene Protective Tapes 3M™ Polyethylene Protective Tapes 4193-EZ is an easy (EZ) unwind polyethylene tape with a very high-tack adhesive system.Information provided by 3M |
|||
Tensile Strength at Break | 1.70 MPa | 247 psi | ASTM D882 |
3M 4F79 Fire Retardant Polyethylene Carpet Protective Tape 3M™ Fire Retardant Polyethylene Carpet Protective Tape 4F79 has a high-tack adhesive system and to help provide temporary protection of carpet during assembly or maintenance of aircraft.Information.. |
|||
Tensile Strength at Break | 1.70 MPa | 247 psi | ASTM D3759 |
3M 5112 Polyethylene Protective Tapes 3M™ Polyethylene Protective Tapes 5112 has a low-tack adhesive system to help provide temporary protection in general industrial applications for man y polished metals, plastics, glass materials an.. |
|||
Tensile Strength at Break | 1.70 MPa | 247 psi | ASTM D3759 |
3M 5125 (Clear) Polyethylene Protective Tapes 3M™ Polyethylene Protective Tapes 5125 has a low-tack adhesive system to help provide temporary protection from abrasion for many polished or painted metals and plastic material with minimum adhesi.. |
|||
Tensile Strength at Break | 1.70 MPa | 247 psi | ASTM D3759 |
3M 5188 (Clear) Polyethylene Protective Tapes 3M™ Polyethylene Protective Tapes 5188 has a high-tack adhesive system to help provide temporary protection of many textured metals and fine matte plastic materials.Information provided by 3M |
|||
Tensile Strength at Break | 1.70 MPa | 247 psi | ASTM D3759 |
3M 5193-EZ Polyethylene Protective Tapes 3M™ Polyethylene Protective Tapes 5193-EZ is an easy (EZ) unwind polyethylene tape with a very high-tack adhesive system.Information provided by 3M |
|||
Tensile Strength at Break | 1.70 MPa | 247 psi | ASTM D3759 |
3M 8179 (Clear) Polyethylene Protective Tapes 3M™ Polyethylene Protective Tapes 8179 has a very high-tack adhesive system to help provide temporary protection for many dissimilar metals, automotive carpeting, carpeted door panels and plastic s.. |