Polymer Property : Tensile Strength at Break = 1.64 MPa
Polymer Property :
Tensile Strength at Break =
1.64 MPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
1.64
MPa
238
psi
510 mm/min; ASTM D412A
PolyOne Elastamax™ HTE 1109 Styrene Butadiene Block Copolymer (SBC) with Mineral Filler (discontinued **)