Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | >= 1.24 MPa | >= 180 psi | ASTM D412 |
Parker Chomerics CHO-SEAL 1287 Conductive Elastomer Conductive Fluorosilicone EMI/EMP Gasket. This material is silver-plated-aluminum-filled fluorosilicone elastomer which provides pressure and environmental sealing as well as high levels of EMI shie.. |
|||
Tensile Strength at Break | >= 1.24 MPa | >= 180 psi | ASTM D412 |
Parker Chomerics CHO-SEAL 1298 EMI Shielding Material Corrosion Resistant EMI Shielding Gasket. Through the use of new proprietary particle painting and elastomer compounding technology, CHO-SEAL® 1298 shielding elastomer offers a six-fold increase in.. |
|||
Tensile Strength at Break | >= 1.24 MPa | >= 180 psi | ASTM D412 |
Parker Chomerics CHO-SEAL 1485 Conductive Elastomer Conductive Elastomer EMI/EMP GasketsInformation provided by Chomerics |
|||
Tensile Strength at Break | 1.24 MPa | 180 psi | ASTM D638 |
ExxonMobil ENABLE™ EN 33330 Adhesive Resin
(discontinued **) Enable EN 33330 is a high flow, 32.5% nBA copolymer suitable for use in hot melt adhesives and sealants.Information provided by ExxonMobil Chemical |
|||
Tensile Strength at Break | >= 1.24 MPa | >= 180 psi | Base Material; ASTM D412 |
Parker Chomerics CHO-SEAL 1287R Reinforced Conductive Elastomer Seal These materials are fabric-reinforced, silver-plated-aluminum filled EMI seals for airframe shielding applications. These seal materials can also be used to maintain surface electrical continuity at.. |
|||
Tensile Strength at Break | 1.24 MPa | 180 psi | ASTM D412 |
Teknor Apex Monprene® MP 2313 Thermoplastic Elastomer Features: Monprene® TPE gels are softer than the shore A range of hardness. Monprene® TPE gels are high strength and high flow elastomers that may be used in the overmolding processes on poly.. |
|||
Tensile Strength at Break | 1.24 MPa | 180 psi | ASTM D412 |
Teknor Apex Monprene® MP-1880 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 1.24 MPa | 180 psi | ASTM D638 |
ExxonMobil EN 33330 Ethylene n-Butyl Acrylate Copolymer Resin Product Description: ExxonMobil EN 33330 is a high flow 32.5% nBA copolymer suitable for use in hot melt adhesives and sealants. Availability: Latin America, North America and South America Additive.. |
|||
Tensile Strength at Break | 1.24 MPa | 180 psi | |
Abatron MasterMold 12-3 Flexible Mold Making Compound Master mold 12-3 is formulated for versatility, high elasticity and strength. It is a 2-component polyurethane system and can be easily spread on any model to produce a smooth bubble-free mold surf.. |
|||
Tensile Strength at Break | 1.24 MPa | 180 psi | |
3M 4026 Double Coated Urethane Foam Tape 3M™ Double Coated Urethane Foam Tapes are conformable foams that offer high shear strength and are available with either a high temperature holding acrylic adhesive system or a rubber adhesive syst.. |
|||
Tensile Strength at Break | >= 1.24 MPa | >= 180 psi | ASTM D412 |
Parker Chomerics CHO-SEAL 1217 Conductive Elastomer Resists highest level of EMP induced current; military gasket of choice in non-corrosive environments; excellent processing for molding and extrusion. Molded and ExtrudedRoHS Compliant Information p.. |