Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength at Break = 0.0850 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 0.0850 MPa
12.3 psi
T Block, 1 in<sup>2</sup> (6.45 cm<sup>2</sup>) Jaw Speed 2 in/min (50 mm/min)
3M 4004 Double Coated Urethane Foam Tape
3M™ Double Coated Urethane Foam Tapes are conformable foams that offer high shear strength and are available with either a high temperature holding acrylic adhesive system or a rubber adhesive syst..