Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 5.55 - 475 J/cm @Temperature -40.0 - -40.0 °C |
10.4 - 890 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 294 J/cm Grade Count:3 |
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an.. |
|||
Izod Impact, Unnotched | 5.55 - 475 J/cm @Thickness 0.800 - 3.17 mm |
10.4 - 890 ft-lb/in @Thickness 0.0315 - 0.125 in |
Average value: 294 J/cm Grade Count:3 |
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an.. |